KR steel plate
KR/R A36|KR A36 STEEL PLATE
KR A36 steel plate, also written as RA36, R A36, KR Grade A36 or market name AH36, is the higher-strength hull structural steel of Korean Register (KR) Rules for the Classification of Steel Ships (IACS UR W11 higher-strength family) with 355 MPa minimum yield, 490-620 MPa tensile strength and Charpy V-notch toughness at 0°C [32°F]. In the grade name, "A" is the toughness class, and "36" refers to the strength level (historically about 36 kgf/mm²); KR mill certificates commonly use the R prefix (RA36), while AH36 is the common IACS market name with "H" for higher strength. Gangsteel, a steel plate exporter, supplies KR A36 / RA36 plates cut to size for shipbuilding, offshore platforms and marine structures.
Data source: Per IACS UR W11 (ordinary/higher-strength hull structural steel) as adopted in KR Class hull structural steel rules. Official mill/certificate grade is typically RA36 (R A36); KR A36 and AH36 name the same class on this site. Verify the current KR Class edition before ordering.
KR A36 / RA36 Chemical Composition (Heat Analysis)
| Element | C | Mn | Si | P | S | Al (acid sol.) |
|---|---|---|---|---|---|---|
| KR A36 / RA36, % | 0.18 max | 0.90-1.60 | 0.10-0.50 | 0.035 max | 0.035 max | 0.015 min |
| Element | Nb | V | Ti | Cu | Cr | Ni / Mo |
| KR A36 / RA36, % | 0.02-0.05 | 0.05-0.10 | 0.02 max | 0.35 max | 0.20 max | 0.40 max / 0.08 max |
Per IACS UR W11 / Korean Register (KR) hull structural steel rules (higher-strength grades). Nb, V and Al grain-refining elements may be used singly or in combination; when used in combination the individual minima do not apply. Where acid-soluble Al is not less than 0.015%, the Si minimum does not apply. Carbon equivalent: Ceq = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15 (%).
Product Analysis (Check Analysis)
IACS UR W11 / KR Class rules do not separately tabulate product (check) analysis limits for higher-strength grades. When product analysis is required, the finished plate shall meet the heat limits subject to ASTM A6/A6M Table A permitted variations (same practice as other IACS societies).
| Element | Heat analysis limit | Product analysis (heat ± A6) |
|---|---|---|
| C | 0.18 max | 0.22 max |
| Mn | 0.90-1.60 | 0.81–1.72 |
| Si | 0.10-0.50 | 0.04–0.56 |
| P | 0.035 max | 0.045 max |
| S | 0.035 max | 0.045 max |
| Al (acid sol.) | 0.015 min | no A6 Table A tolerance; product value not tabulated |
| Nb | 0.02-0.05 | 0.010–0.060 |
| V | 0.05-0.10 | 0.040–0.110 |
| Ti | 0.02 max | 0.03 max |
| Cu | 0.35 max | 0.38 max |
| Cr | 0.20 max | 0.24 max |
| Ni | 0.40 max | 0.43 max |
| Mo | 0.08 max | 0.09 max |
Per IACS UR W11 / KR Class hull structural steel rules. Product analysis applies only when specified; for a range, results may not vary both above and below it.
KR A36 / RA36 Mechanical Properties
| Grade | Yield strength, min | Tensile strength | Elongation, min |
|---|---|---|---|
| KR A36 (RA36) | 355 MPa [51 ksi] | 490-620 MPa [71-90 ksi] | 21% |
Per IACS UR W11 / KR Class hull structural steel rules. Yield and tensile values apply for the full thickness range covered by the grade (typically up to 100 mm for these ship plates).
Charpy V-Notch Impact Requirements (0°C [32°F])
| Thickness | Test temperature | Longitudinal, avg min | Transverse, avg min |
|---|---|---|---|
| t≤50 mm | 0°C [32°F] | 34 J | 24 J |
| 50<t≤70 mm | 0°C [32°F] | 41 J | 27 J |
| 70<t≤100 mm | 0°C [32°F] | 50 J | 34 J |
Per IACS UR W11 / KR Class hull structural steel rules. Average of three full-size Charpy V-notch specimens; not more than one value below the average and none below 70% of it. Longitudinal values shown; transverse values apply when required by the rules or purchase order. Thicker plates (above 100 mm) may be supplied by agreement with adjusted impact requirements.
Delivery Condition and Deoxidation
Deoxidation: Killed, fine-grain practice. Delivery condition: A-class (R A36 / AH36) grades may be as-rolled, controlled rolled, normalized or TMCP depending on thickness; thicker plates usually N or TMCP. Optional extras by agreement include ultrasonic testing, Z-direction (Z15/Z25/Z35) through-thickness testing and third-party KR survey.
Thickness Coverage
Higher-strength KR A/D/E/F 32/36/40 plates are commonly supplied from about 6 mm to 100 mm thick (up to 150 mm by agreement). Width 1500-4000 mm and length 6000-18000 mm are typical.
Equivalent Steel Grades of KR A36
| Society / Standard | Equivalent grade |
|---|---|
| KR (Korean Register) | KR A36 / RA36 (AH36) |
| LR (Lloyd's Register) | LR AH36 steel plate |
| ABS | ABS AH36 steel plate |
| CCS | CCS AH36 steel plate |
| ASTM A131/A131M | ASTM A131 AH36 steel plate |
| GL | GL AH36 steel plate |
| DNV | DNV A36 steel plate |
| BV | BV AH36 steel plate |
| NK | NK A36 steel plate |
| RINA | RINA AH36 steel plate |
IACS member societies harmonize ordinary and higher-strength hull grades under UR W11; dual certification (for example KR + ABS, or KR + ASTM A131) is common when ordered that way.
FAQ about KR A36 / RA36 Steel Plate
What is KR A36 (RA36) steel plate?
It is a higher-strength hull structural steel under Korean Register (KR) Rules for the Classification of Steel Ships (IACS UR W11), with 355 MPa minimum yield, 490-620 MPa tensile strength and Charpy toughness at 0°C [32°F]. The mill certificate grade is typically RA36 (R A36); KR A36 and market name AH36 refer to the same strength/toughness class.
What does KR A36 / RA36 / AH36 stand for?
KR is Korean Register. The R prefix on the mill grade (RA36 / R A36) is the KR designation. The letter A is the toughness class (Charpy at 0°C [32°F]), and 36 is the strength level (historically about 36 kgf/mm², now 355 MPa min yield). AH36 adds "H" for higher strength in common IACS market naming.
What is the yield strength of KR A36?
Minimum 355 MPa (51 ksi), tensile 490-620 MPa (71-90 ksi), elongation about 21% min.
What is the impact test temperature for KR A36 / RA36?
Charpy V-notch at 0°C [32°F]. Longitudinal average minima are 34 J up to 50 mm, 41 J for 50-70 mm and 50 J for 70-100 mm.
What is the difference between KR A36 and other 36-class grades?
Same 355 MPa strength class. NK A36 (KA36) at 0°C [32°F]; NK D36 (KD36) at -20°C [-4°F]; NK E36 (KE36) at -40°C [-40°F]; NK F36 (KF36) at -60°C [-76°F]. Delivery condition follows the toughness letter rules.
What is the difference between KR A36 and NK A32?
Same A-class toughness (Charpy at 0°C [32°F]). KR A36 is strength class 36 (355 MPa min yield); NK A32 is strength class 32 (315 MPa min yield).
Is KR A36 the same as ABS AH36 or LR AH36?
Requirements are essentially harmonized under IACS UR W11. ABS AH36, LR AH36, DNV A36, BV AH36 and ASTM A131 AH36 (where listed) are counterparts; dual certification is common when ordered with the required surveys.
Is KR A36 weldable?
Yes. Controlled carbon and Ceq give good weldability; preheat may be required for thick sections depending on Ceq and restraint.
What heat treatment is required for KR A36?
A-class (R A36 / AH36) grades may be as-rolled, controlled rolled, normalized or TMCP depending on thickness; thicker plates usually N or TMCP.
What thickness is available for KR A36?
Typical supply is about 6-100 mm thick (up to 150 mm by agreement), 1500-4000 mm wide and 6000-18000 mm long.
Other KR Steel Plate Grades
KR Grade A steel plate | KR Grade B steel plate | KR Grade D steel plate | KR Grade E steel plate | KR A32 steel plate | KR A40 steel plate | KR D36 steel plate | KR D40 steel plate | KR E32 steel plate | KR E36 steel plate | KR E40 steel plate | KR F32 steel plate | KR F36 steel plate | KR F40 steel plate | KR D63 / RD63 steel plate
Equivalent Class Society Grades
KR A36 / RA36 (AH36) corresponds to the same grade under the other IACS member classification societies and ASTM A131: LR AH36 steel plate, ABS AH36 steel plate, CCS AH36 steel plate, ASTM A131 AH36 steel plate, GL AH36 steel plate, DNV A36 steel plate, BV AH36 steel plate, NK A36 steel plate, RINA AH36 steel plate.
-
R A|KR Grade A STEEL PLATE
KR Grade A (IACS ordinary-strength hull steel) [queue key KR-Grade-A-Plate]: identity, chemistry, mechanical pr
-
KR/R F70|KR F70 STEEL PLATE
KR F70 (RF70) shipbuilding steel plate: 690 MPa yield, 770-940 MPa tensile, Charpy at -60C, chemistry and equiv
-
KR/R E36|KR E36,KR Grade EH36 S
KR E36 (RE36) shipbuilding steel plate: 355 MPa yield, 490-620 MPa tensile, Charpy at -40C, chemistry and equiv
-
KR/R E32|KR E32,KR Grade EH32 S
KR E32 (RE32) shipbuilding steel plate: 315 MPa yield, 440-590 MPa tensile, Charpy at -40C, chemistry and equiv