CCS DH36 (also written CCS/DH36, CCS Grade DH36, CCS D36 or DH36 steel plate) is a higher-strength hull structural steel plate certified by the China Classification Society (CCS) to CCS Rules for Materials and Welding (2024), Part 1, Chapter 3, Section 3. The figure 36 is the strength level (minimum yield 355 MPa, tensile 490–630 MPa) and the letter D sets the Charpy V-notch test temperature of −20°C. The steel is killed and fine-grain treated, and the grade corresponds to DH36 in IACS UR W11 and DH36 in ASTM A131.

Gangsteel, a steel plate exporter, supplies CCS DH36 plate with CCS class certificates; the requirements below are taken directly from the current CCS rules.

Related CCS grades: CCS AH36 steel plate, CCS EH36 steel plate, CCS FH36 steel plate, CCS DH32 steel plate, CCS DH40 steel plate.

CCS DH36 chemical composition

CCS DH36 chemical composition, heat (ladle) analysis, %
Element Heat analysis
C ≤ 0.18
Mn 0.90–1.60 (≥ 0.70 for t ≤ 12.5 mm)
Si ≤ 0.50
P ≤ 0.035
S ≤ 0.035
Al (acid soluble) ≥ 0.015
Nb 0.02–0.05
V 0.05–0.10
Ti ≤ 0.02
Nb + V + Ti ≤ 0.12
Cu ≤ 0.35
Cr ≤ 0.20
Ni ≤ 0.40
Mo ≤ 0.08

 

Source: CCS Rules for Materials and Welding (2024), Part 1, Chapter 3, Table 3.3.2.1. Al, Nb and V are grain-refining elements: when used in combination, the individual minimum contents do not apply. Total Al ≥ 0.020% may be reported instead of acid-soluble Al. TMCP plates must also meet the Ceq limits below. CCS specifies the chemical composition as a heat (ladle) analysis only; the Rules give no product (check) analysis tolerances for these plates, so no product-analysis column is shown. If a product analysis is required, agree the tolerances in the order.

CCS DH36 mechanical properties and impact test

CCS DH36 tensile and Charpy V-notch requirements
Grade Yield ReH min (MPa) Tensile Rm (MPa) Elongation A5 min (%) Test temp. KV avg min, t ≤ 50 mm, L / T (J) 50 < t ≤ 70 mm, L / T (J) 70 < t ≤ 150 mm, L / T (J)
CCS DH36 355 490–630 21 −20°C 34 / 24 41 / 27 50 / 34

Source: CCS Rules for Materials and Welding (2024), Part 1, Chapter 3, Table 3.3.4.3. L = longitudinal, T = transverse. Impact tests are normally made longitudinally; transverse values must be guaranteed by the mill.

CCS DH36 maximum carbon equivalent for TMCP plates
Thickness t ≤ 50 mm 50 < t ≤ 100 mm 100 < t ≤ 150 mm
Ceq max (%) 0.38 0.40 0.42

Ceq = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15, from the ladle analysis (Table 3.3.2.3(1)). For non-TMCP plates a Ceq limit may be agreed.

CCS DH36 thickness range and delivery condition

The CCS rules for CCS DH36 cover plates and wide flats up to 150 mm thick (sections and bars up to 50 mm). The permitted supply condition (as-rolled, controlled rolled, normalized or TMCP) depends on thickness and on the grain-refining elements used; see Table 3.3.3.1. The required Charpy energy increases above 50 mm and again above 70 mm.

CCS DH36 equivalent grades

CCS DH36 equivalent grades of other classification societies
Standard / society Equivalent grade
IACS UR W11 DH36
ABS AB/DH36
DNV VL D36
LR LR DH36
BV BV DH36
ASTM A131 DH36
China GB/T 712 DH36

The IACS member societies use the same unified requirements, so these grades match in chemistry and properties. A plate still needs the certificate of the vessel’s own class society; one plate can carry dual or multiple class certification only when each society’s surveyor witnesses the tests.

CCS DH36 FAQ

What does DH36 mean?

D sets the toughness grade (Charpy test at −20°C), H means higher strength, and 36 is the strength level: minimum yield 355 MPa.

What is the yield strength of CCS DH36?

Minimum 355 MPa, tensile strength 490–630 MPa and minimum elongation 21%.

What is the impact test temperature of CCS DH36?

−20°C. Minimum average energy is 34 J longitudinal / 24 J transverse up to 50 mm, 41/27 J for 50–70 mm and 50/34 J for 70–150 mm.

What is CCS DH36 equivalent to?

DH36 of IACS UR W11, ABS AB/DH36, DNV VL D36, LR and BV DH36, ASTM A131 DH36 and GB/T 712 DH36.

What is the difference between AH36, DH36, EH36 and FH36?

They share the same chemistry limits (FH has tighter C, P and S limits, an N limit and a higher Ni allowance) and the same strength. Only the Charpy test temperature changes: 0°C (A), −20°C (D), −40°C (E) and −60°C (F).

What is the difference between CCS DH36 and ABS DH36?

Both are the same IACS UR W11 grade, so in practice they are interchangeable technically; the difference is the class certificate. Note: CCS gives tensile 490–630 MPa, while ABS lists 490–620 MPa.

What is the carbon equivalent (CEV) of CCS DH36?

For TMCP plates Ceq must not exceed 0.38% up to 50 mm, 0.40% for 50–100 mm and 0.42% for 100–150 mm. For other conditions a Ceq limit may be agreed with the buyer.

What thickness range does CCS cover for DH36?

Plates and wide flats up to 150 mm; sections and bars up to 50 mm.

Equivalent steel grade of CCS/DH36

DNV

GL

LR

BV

ABS

NK

KR

RINA

NV D36

GL-D36

LR/DH36

BV/DH36

ABS/D36

K D36

R D36

RI/D36

If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.

Related steel grades: CCS/AH36, CCS/EH36, CCS/FH36, CCS/DH40

 

CCS Steel Plate Grade

General Strength

CCS/A

CCS/B

CCS/D

CCS/E

High Strength

CCS/A32

CCS/D32

CCS/E32

CCS/F32

CCS/A36

CCS/D36

CCS/E36

CCS/F36

CCS/A40

CCS/D40

CCS/E40

CCS/F40

Extra Strength

CCS/A420

CCS/D420

CCS/E420

CCS/F420

CCS/A460

CCS/D460

CCS/E460

CCS/F460

CCS/A500

CCS/D500

CCS/E500

CCS/F500

CCS/A550

CCS/D550

CCS/E550

CCS/F550

CCS/A620

CCS/D620

CCS/E620

CCS/F620

CCS/A690

CCS/D690

CCS/E690

CCS/F690

 

ASTM equivalent: ASTM A131 DH36 steel plate

LR equivalent: LR DH36 steel plate

Other Products